Heat effected zone in unburned, antimony trioxide containing plasticised PVC

Al-Mosawi, Ali I. and Marossy, Kálmán (2018) Heat effected zone in unburned, antimony trioxide containing plasticised PVC. ÉPÍTŐANYAG – JOURNAL OF SILICATE BASED AND COMPOSITE MATERIALS, 70 (3). pp. 86-89. ISSN 0013-970X (nyomtatott); 2064-4477 (online)

[img]
Preview
Text
Heat Effected Zone in Unburned, Antimony Trioxide Containing Plasticised PVC.pdf
Available under License Creative Commons Attribution Non-commercial.

Download (2MB) | Preview

Abstract

What are the structural changes in the PVC layer located directly under the flame zone which is exposed to high temperatures without burning? We will try to explain in this article what actually happens in this layer, which we called heat affected zone. The layers were tested both with and without antimony trioxide (ATO or Sb2O3) flame retardant additive. Results obtained from Scanning Electron Microscopy (SEM) for the heat affected zone of the samples after Limited Oxygen Index (L.O.I) test and compared with the samples before this test showed that there was a significant decrease in the chlorine content in the PVC structure accompanied by a significant increase in the carbon content. We suppose that this early dehydrochlorination improves the efficiency of Sb2O3.

Item Type: Article
Uncontrolled Keywords: Plasticised PVC; HAZ; L.O.I.; SEM; EDS
Subjects: T Technology / alkalmazott, műszaki tudományok > TP Chemical technology / vegyipar, vegyészeti technológia
Depositing User: Mr. Ali Ibrahim Moslem Maeeni
Date Deposited: 11 May 2021 06:44
Last Modified: 11 May 2021 06:44
URI: http://real.mtak.hu/id/eprint/125170

Actions (login required)

Edit Item Edit Item